Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of NORYL GTX™ Resin GTX910 - Europe - (PPE+PA*) - Saudi Basic Industries Corporation (SABIC)

Material Data Center offers the following functions for NORYL GTX™ Resin GTX910 - Europe:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Noryl GTX datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informations produit
NORYL GTX™ 910 resin is non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). NORYL GTX910 resin exhibits excellent chemical resistance and is an excellent candidate for automotive applications such as plastic/metal hybrid components, rail extensions, crash cans, wheel covers, and energy absorbers.
Caractéristiques des transformations/physiquesValeurUnitéNorme du test
ISO Data
Indice de fluidité à chaud en volume, MVR 10 cm³/10min ISO 1133
Température 280 °C -
Charge 5 kg -
Propriétés mécaniquesValeurUnitéNorme du test
ISO Data
Module en traction 2200 MPa ISO 527
Contrainte d'écoulement 55 MPa ISO 527
Déformation au seuil d'écoulement 8 % ISO 527
Contrainte à la rupture 50 MPa ISO 527
Déformation à la rupture 25 % ISO 527
Module de flexion 1900 MPa ISO 178
Résistance au choc Charpy (entaillé), +23°C 25 kJ/m² ISO 179/1eA
Résistance au choc Charpy (entaillé), -30°C 12 kJ/m² ISO 179/1eA
Résistance au choc Izod (entaillé), +23°C, 4mm 25 kJ/m² ISO 180/1A
Résistance au choc Izod (entaillé), -30°C, 4mm 12 kJ/m² ISO 180/1A
Ball indentation hardness 115 MPa ISO 2039-1
Propriétés thermiquesValeurUnitéNorme du test
ISO Data
Température de ramolliss. Vicat, A 238 °C ISO 306
Température de ramolliss. Vicat, B 195 °C ISO 306
Température de ramolliss. Vicat, 120°C/h 50N 195 °C ISO 306
Coeffic. de dilatation therm. linéique, parallèle 90 E-6/K ISO 11359-1/-2
Coeffic. de dilatation therm. linéique, perpend. 90 E-6/K ISO 11359-1/-2
Conductivité thermique 0.23 W/(m K) DIN 52616
Propriétés diversesValeurUnitéNorme du test
Absorption d'eau 3.5 % Sim. to ISO 62
Absorption d'humidité 1 % Sim. to ISO 62
Masse volumique 1100 kg/m³ ISO 1183
Recommandations pour la transformation Moulage par injectionValeurUnitéNorme du test
Pré-séchage - température 100 - 120 °C -
Pré-séchage - temps 2 - 3 h -
L'humidité de traitement ≤0.07 % -
Température de la matière fondue 280 - 310 °C -
Température du moule 80 - 120 °C -
Température - Zone d'alimentation 60 - 80 °C -
Zone 1 260 - 280 °C -
Zone 2 270 - 290 °C -
Zone 3 280 - 300 °C -
Caractéristiques
Transformation
Moulage par injection
Applications
Automobile
Disponibilité régionale
Europe
Conditions générales
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.